US PATENT SUBCLASS 374 / 26
.~.~ Of molten metal (e.g., carbon content)


Current as of: June, 1999
Click HD for Main Headings
Click for All Classes

Internet Version by PATENTEC © 1999      Terms of Use



374 /   HD   THERMAL MEASURING AND TESTING

16  DF  TRANSFORMATION POINT DETERMINATION (E.G., DEW POINT, BOILING POINT) {6}
25  DF  .~ By thermal arrest (e.g., time-temperature curve) {1}
26.~.~ Of molten metal (e.g., carbon content)


DEFINITION

Classification: 374/26

Of molten metal (e.g., carbon content):

(under subclass 25) Subject matter for determining a thermal arrest point of a molten metal.

(1) Note. The thermal arrest point is often used to determine carbon content of the molten metal.

SEE OR SEARCH THIS CLASS, SUBCLASS:

139+, for molten metal temperature measurement, in general.